Dear All, I`m trying to refine the synchrotron data of BaTiO3 powder. In my case, i believe that Ti has two valance states, 3+ and 4+. Since the x rays are scattered from the electrons, Ti 3+ and Ti 4+ should act as different scatterers. I want to add both Ti 3+ and Ti 4+ to the lattice. I think, when i add the Ti atoms to the lattice, it is treated as Ti 4+. Is there a way to add Ti 3+ ions to the lattice? Or my argument does not make any sense?
Happy Refinements Vahit ========================================================================= Vahit Atakan Ph.D student Rutgers, The State University of New Jersey Department of Ceramic and Materials Science & Engineering Room CCR 143 607 Taylor Road Piscataway, NJ 08855-0909 732-445-5564 732-445-6264 (fax) [EMAIL PROTECTED] -----Original Message----- From: Brian H. Toby [mailto:[EMAIL PROTECTED] Sent: Wednesday, March 02, 2005 4:06 PM To: [email protected] Brian H. Toby wrote: > At present, to my knowledge, there is exactly one program that can be > used to read & plot powder diffraction data from these CIFs: pdCIFplot This turns out to be wrong. CMPR can also do this (http://www.ncnr.nist.gov/xtal/software/cmpr/). My apologies to the author of that program. Brian