Title: Message
Gerard,
In GSAS there is a GENLES "print" option that will give the covariance terms larger than +/- 0.5 in the list file. There aren't as many large ones as you might think apart from the various background terms.
Bob Von Dreele
 
 

R.B. Von Dreele

IPNS Division

Argonne National Laboratory

Argonne, IL 60439-4814

 

-----Original Message-----
From: Gerard, Garcia S [mailto:[EMAIL PROTECTED]
Sent: Thursday, May 05, 2005 8:56 AM
To: [EMAIL PROTECTED]
Cc: [email protected]
Subject: correlation matrix

Dear all,
 
I suspect that in my rietveld refinements i have severe correlation problems. Is there any way of having a look at the matrix where this correlations are stood out?
 
Thanks
 
Gerard

Reply via email to