Title: Message
Dear Don, I observed too that in Expgui multiplicity column is not always readily updated when one changes position/multiplicity. To have an update also in Expgui I usually run Expedt (GSAS interface) then I go to the "list atom menu" (i.e. sequence L A L), where I can see the true and updated list of multiplicities; after if I exit GSAS and come back to Expgui I see the updated list of multiplicities.
Good job,
Marco
 
----- Original Message -----
Sent: Tuesday, May 17, 2005 6:31 AM
Subject: mismatch between ICSD cif file and GSAS

Drs. Payzant, Larson, & Von Dreele,

Thanks for your quick response. 

 

After 1/8 offset, it appears that the pattern from live plot is a good match to ICSD-generated pattern, which basically solved my problem.  I am very happy and grateful.

 

There is still a little problem.  The multiplicity column did not change at all (in EXPGUI).  Please explain.

 

Best regards

Don

 

-----Original Message-----
From: Von Dreele, Robert B. [mailto:[EMAIL PROTECTED]
Sent:
Monday, May 16, 2005 9:30 AM
To: [email protected]
Subject: RE: mismatch between ICSD cif file and GSAS

 

Don,

As Allen Larson noted GSAS only uses the 2nd setting for space groups that have two (e.g. F d 3 m) so that he inversion center is placed at the origin. The eta alumina structure you have is for the 1st setting. To convert from 1st to 2nd subtract 1/8,1/8,1/8 from all xyz. That will fix the structure factors & the site multiplicity problems.

Bob Von Dreele

 

 

R.B. Von Dreele

IPNS Division

Argonne National Laboratory

Argonne, IL 60439-4814

 

-----Original Message-----
From: Donald Wang [mailto:[EMAIL PROTECTED]
Sent:
Sunday, May 15, 2005 9:31 PM
To: [email protected]
Subject: mismatch between ICSD cif file and GSAS

Dear all,

 

I have a puzzle here.  I have been learning GSAS for a while but still at a relatively low level.  I am trying to calculate % of glass phase in a plasma sprayed alumina coating (eta alumina, ISCD #39104, space group Fd-3M, 227).  The structure is copy-pasted as below:

 

 

Atom    #          OX        SITE      x           y             z           SOF            H        ITF(B)   

 O         1          -2          32 e     0.37        0.37        0.37        1.               0              3.

 Al        1           +3        8 a       0.25        0.25        0.25        0.503         0              3.

 Al        2           +3        48 f      0.25        0             0            0.083         0              3.

 Al        3           +3       16 d      0.625      0.625       0.625      0.564         0              3.

 Al        4           +3       16 c      0.125     0.125        0.125       0.27          0              3.

 

 

However, when this CIF file is imported into GSAS (using EXPGUI), EXPGUI shows the following corresponding multiplicity

32

32

32

8

8

 

and GSAS-simulated XRD pattern is much different from the one generated from ICSD.  Please help on this mismatch between ICSD and GSAS-EXPGUI. 

 

 

Many thanks in advance

Don

 

Donald Wang

University of Connecticut

 

Reply via email to