Dear Rietvelders,
I am working with few molybdenum chalcogenides
(hexagonal) and I have noticed that when I
measure it (micronic powder in a flat sample holder) in Bruker D8 (Bragg
Brentano) with Gobbel mirror, the major peak at around 13 2Th is twice intense
of doing the same measurement in Bruker D8 without Gobbel mirror while the rest
of the pattern is the same. the refinement (fullprof) is much better for the
sample measured with the mirror.
my questions is:
1. what could be the reasons for this difference?
(absorption??)
2. how can I overcome this problem? (sample
preparation, refinement)
Thanks in advance for your help
Eli Lancry
Chemistry department Bar-Ilan University, Ramat Gan ISRAEL Phone: 972-(0)3-5317665/8169 Mobile: 972-(0)54-2212717 Fax: 972-(0)3-5351250 E-mail: [EMAIL PROTECTED] |
- Gobbel Mirror eli lancry