Hello everybody!
I am trying to convert a GSAS ESD file to a GSAS STD file (to use in
FullProf). I successfully used the program "Convert" to do so, but when I
plotted my data, I realized that Convert erased all my numbers after the
decimal point, leading to very crude patterns with very obvious steps (this
is high-pressure data, so for higher pressures, the overall intensity
differences are not all that high). Does anybody know a simple solution to
this problem, like a different conversion program, or a way to get Convert
to keep the 2 decimal places?
Cora
*******************************************
Dr. Cora Lind
WO 2262
Department of Chemistry, MS 602
University of Toledo
Toledo, OH 43606-3390
Phone: (419) 530-1505 (W) (419) 472-8364 (H) (607) 592-4650 (Cell - when
traveling)
Fax: (419) 530-4033 (W) (419) 472-8364 (H)
e-mail: [EMAIL PROTECTED]
*******************************************