Stanislav Ferdov schrieb:

Dear All,

I am trying to refine the structure of a porous
vanadoslicate, however FullProf does not recognize the
scattering coefficient of V4+. Does somebody know how
I could modify the pcr file in order to work with V4+?
Well, there just is no scattering factor for V+4 in the internal list, and I'm not sure there is some at all. However, V+3 and V+5 ARE in the list. I would suggest just
defining a mixed occupation of those.

Daniel Toebbens