At 13:00 25/10/2006, you wrote: >Do any of you have available the ICSD Card for Orthorombic (martensite) NiTi? >In case, could you send it to me (or some indications on how to find it)?
That's easy. You can find it from ICSD on-line http://icsdweb.fiz-karlsruhe.de/ (if you have an ICSD access license :-)) Otherwise try Google. BTW I think martensite NiTi is monoclinic not orthorhombic. Alan. _____________________________________________________________ Dr Alan Hewat, ILL Grenoble, FRANCE<[EMAIL PROTECTED]>fax+33.476.20.76.48 +33.476.20.72.13 (.26 Mme Guillermet) http://www.ill.fr/dif/people/hewat/ _____________________________________________________________