Dear All

As far as I know the axes x, y and z output by mustrplot are defined as 
follows: x||a*, y||c* x a*, z||c. Is it possible in principle to transform the 
coordinates in such a way that x||a, y||b, z||c (if yes, how is this done)? 
I.e. to display the microstrain in real space. This would ease the description 
of structure-strain relations.

Thank you for your comments.

Franz Werner

Technische Universitaet Wien