Good evening,
I have two questions for FullProf users:
 
1. If I want to refine the sample transparency (Sysin), should I put also
the absorption coefficient (muR)? What's happened mathematically when muR
remains to be zero? (I saw that SYSIN = 1/(2mR) but this parameter
apparently can be refined..)
2. From FullProf manual I get that absorption coefficient is taken into
account only for cylindrical samples. How the program knows about the sample
shape if I use for example synchrotron settings?
 
Thank you very much!
Irina
 
*****************************
Irina Pozdnyakova
CNRS-CRMHT
1d, avenue de la Recherche Scientifique
45071 ORLEANS CEDEX 2
Tel 02 38 25 76 93
Fax 02 38 63 81 03
*******************************
 

Reply via email to