Dear all,

Sorry I replied directly back, rather than to the list - problems of webmail, not being able to see everything clearly.

Anyway, I don't think there is a one step method for analysing/reading Bruker RAW format files unless you purchase their software - commercial sense.

The program I know which deals successfully with Bruker and converts to GSAS (good test for conversion) with minimal hitches is ConvX.

http://www.ccp14.ac.uk/ccp/web-mirrors/convx/

It can convert Bruker to many other formats too. Then the data can be viewed using programs such as Origin, Matlab, etc commercial software or there is the free program LAMP which can give you glossy looking 3D images. There are possibly others; can whoever knows of alternative free 3D viewing packages let me know please.

http://www.ill.fr/data_treat/lamp/front.htm

Can someone please tell me the quickest download website for LAMP?

Once again though you will have to convert the data before hand to XY.

Alternatively purchase TOPAS Academic which is one half of Bruker's TOPAS Rietveld program. That can read RAW Bruker files without any problems and I'm sure can display multi pattern. (?)

Professor Knowles I see you are from the UCL Eastman Dental Institute, if you want any help/demonstrations feel free to come over to UCL Chemistry or I can walk over to Gray's Inn road.

Regards
William Bisson

----- Forwarded message from [EMAIL PROTECTED] -----
    Date: Mon, 15 Jan 2007 16:33:23 +0000
    From: [EMAIL PROTECTED]
Reply-To: [EMAIL PROTECTED]
 Subject: Re:
      To: ugez323 <[EMAIL PROTECTED]>

Dear Professor Knowles,

Use the program ConvX

http://www.ccp14.ac.uk/ccp/web-mirrors/convx/

Which can convert Bruker RAW to many formats for use with other programs

Regards
William Bisson

Quoting ugez323 <[EMAIL PROTECTED]>:

Dear All

We have a Bruker D8 and are collecting multiple datasets for material such
as cements against time. We use the Bruker's EVA software for 3D plotting of
the data and also contour type plots.

Is there any freeware available that will read in RAW format files

Thanks

Professor J.C. Knowles BSc(hons), PhD, FIMMM, CEng, FRSC, CSci
Professor of Biomaterials Science
Head of Division of Biomaterials and Tissue Engineering,
UCL Eastman Dental Institute,
University College London,
256 Gray's Inn Road,
London WC1X 8LD. UK.
Tel +44 (0)207 915 1189
Fax +44 (0)207 915 1227
Mobile 07785 313615
Skype Me
Editor, Journal of Biomaterials Applications
Email [EMAIL PROTECTED]
Eastman website; http://www.eastman.ucl.ac.uk
Personal website; http://www.eastman.ucl.ac.uk/~jknowles
This email represents the views of the sender alone and must not be
construed as representing the views of the Eastman Dental Institute. It may
contain confidential information and may be protected by law as a legally
privileged document and copyright work. Its content should not be disclosed
and it should not be given or copied to anyone other than the person(s)
named or referenced above. If you have received this email in error, please
contact the sender.







----- End forwarded message -----

Reply via email to