Thanks a lot! I will think about it carefully.
Iris

From: "Von Dreele, Robert B." <[EMAIL PROTECTED]>
Reply-To: [email protected]
To: <[email protected]>
Subject: RE:   RE:   RE: Re: about format convert
Date: Tue, 3 Apr 2007 07:52:43 -0500

Hi,
A few important points:
1) Removing Ka2 from the powder pattern is not necessary for running GSAS
(or Fullpoof for that matter). Both represent the Ka1-Ka2 doublet quite nicely. More important, most Ka2 stripping routines can adversly distort the data messing up the result from a Rietveld refinement - I advise not doing it!
2) Newest version of GSAS does not use the old "direct access" format for
raw powder data, making cnvfile no longer necessary.
Bob Von Dreele

________________________________

From: Duncan, Jo [mailto:[EMAIL PROTECTED]
Sent: Tue 4/3/2007 7:30 AM
To: [email protected]
Subject: RE: RE: Re: about format convert



It is an option in GSAS. In PCGSAS: Setup -> Cnvfile

jo

-----Original Message-----
From: liu ?? [mailto:[EMAIL PROTECTED]
Sent: 03 April 2007 13:16
To: [email protected]
Subject: RE: Re: about format convert

Excuse me, i have not heard of it. is it a software?

Iris


>From: "Duncan, Jo" <[EMAIL PROTECTED]>
>Reply-To: [email protected]
>To: <[email protected]>
>Subject: RE:   Re: about format convert
>Date: Tue, 3 Apr 2007 12:44:29 +0100
>
>Have you tried Cnvfile ?
>
>I've never had to use it but I hear it works wonders!
>
>Jo
>
>-----Original Message-----
>From: liu ?? [mailto:[EMAIL PROTECTED]
>Sent: 03 April 2007 12:03
>To: [email protected]
>Subject: Re: about format convert
>
>yes, i can save in "GSAS .DAT"format, but i can not import this format
into
>the GSAS.  The software always reminds me it is not the proper format.
Can
>you give me further advice?
>
>Thanks in advance!
>Iris
>
>
> >From: "Cheng Dong" <[EMAIL PROTECTED]>
> >Reply-To: [email protected]
> >To: "[email protected]" <[email protected]>
> >Subject: Re: [??????????????]about format convert
> >Date: Tue, 3 Apr 2007 15:19:23 +0800
> >
> >After you eliminate the alpha2 using the PowerX, simply save it in
GSAS
>format by Selecting "Save data" from the "File" menu and choose the
"GSAS
>.DAT" with PowderX.
> >
> >Cheng Dong
> >
> > >Dear all,
> > >
> > >I have a little problem and hope someone to help me.
> > >
> > >After I used the PowerX to remove the eliminate the alpha2, I got
the
>.xrd
> > >format files. How cam i convert them into the right format which i
can
>used
> > >in GSAS?  I have tried several softwares, none of them has this
>function.
> > >
> > >Looking forward to your letters.
> > >
> > >best regards,
> > >Iris
> > >
> > >_________________________________________________________________
> > >??????????????- MSN Hotmail? http://www.hotmail.com
<http://www.hotmail.com/>
> >
>
>_________________________________________________________________
>???? MSN Explorer:   http://explorer.msn.com/lccn
>
>

_________________________________________________________________