Hi All,
1. I am facing some problem in calculating the Lorentzian and Gaussian FWHM,
and mixing parameters from the refined values in gsas. I tried calculating,
using the equations given in the gsas manual, but the FWHM which I was getting
has a large deviation with the FWHM in the '.rfl' file and I hope that my value
is not at all reasonable. I used the profile function 2 (TCH function with
anisotropy terms included) in gsas. Please suggest me the procedure and the
parameters which are exactly responsible for finding them.
2. By assuming Cauchy distribution for size and Gaussian distribution for
strain, Can I take GV and GW, and LY as the fixed parameters because, the
parameter GU is
the Strain component in the Cagliotti eqn. and LX is the Size component in the
Lorentzian equations.
Kindly, suggest me in solving this.
Thanks in advance.
Regards
Raju