Laurent, you may find this review paper useful:
Levin, I., Brandon, D., 1998: Metastable alumina polymorphs: crystal structures and transition sequences. J. Am. Ceram. Soc. 81 (8), 1995-2012.
Juro Majzlan On 06.09.2007, at 15:09, Laurent Favaro wrote:
Dear Rietvelders, I am searching for the structure of various transition aluminas (especially rho, eta, khi, gamma, delta and sigma) to perform ab-initio calculations of their infrared spectra. Could you, please, inform me about those structures ? Best regards, Dr L. Favaro Laboratoire LEMHE Université Paris-Sud Orsay, France