Hi All

I know this doesn't have direct application to rietveld work (well, I will be
using it), but I am doing time-resolved powder XRD precipitation experiments in
hydrothermal aqueous solutions using 1mm OD sapphire capillaries, a furnace
mounted to our XRD and epoxy.  I am curious whether there are other sealants
people have used other than epoxy, or what type of epoxies people prefer.  I'm
looking at temperatures up to 300C.

Thanks for any help

Cheers
Lachlan

- -
Lachlan C.W. MacLean, PhD.
Center for Environmental
Kinetics Analysis
413 Deike Building
Pennsylvannia State
University
University Park, PA  16801