Yes it does. One way is to add the command adps at the end of the line site E.g. site Pb1 x 0.23 y 0.15 z 0.28 occ Pb 1 adps
Mike Glazer -----Original Message----- From: Peter Tzvetkov [mailto:[EMAIL PROTECTED] Sent: 10 December 2007 18:28 To: [email protected] Subject: Topas Dear all, Does anyone knows if Topas can refine anisotropic temperature factors? I couldn't find information about this in the technical reference. Maybe I've missed something? Best, Peter Tzvetkov Institute of General and Inorganic Chemistry Bulgarian Academy of Sciences