Dear Maria, We are developing standard materials for XRD and can help you. You can write directly to my e-mail for details. Luis Quoting "Chrysochoou, Maria" <[EMAIL PROTECTED]>:
Does anyone have a suggestion for a vendor that has crystalline corundum, zincite and/or rutile to use as internal standards except NIST? The SRM standards are very expensive for very little
quantity.
Thank you, Maria Chrysochoou Assistant Professor Department of Civil and Environmental Engineering University of Connecticut Storrs CT 06269 E-Mail: [EMAIL PROTECTED] Tel.: (860) 486 3594 Fax: (860) 486 2298
-- Dr. Luis Gallego Martinez Comissão Nacional de Energia Nuclear Instituto de Pesquisas Energéticas e Nucleares Centro de Ciência e Tecnologia de Materiais Av. Prof. Lineu Prestes 2242 Cidade Universitária - USP São Paulo - SP - Brasil - CEP:05508-000 Tel: + 55 11 3133-9222 Fax: 3133-9276 [EMAIL PROTECTED] www.ipen.br