Dear all,
Could you please help me to translate this chunk of the correlation matrix?
HSCL is the histogram scale factor
PF profile coefficients
RMii lattice parameters
ABS?
UISo thermal parameters
how do i interpret the numbers? and the signs? how strongly correlated these
variables are?
regards
The correlation matrix terms greater than 0.50 are
1 1UISO-1 2UISO 5011 3UISO 687 1HSCL 801
1 2UISO- 1HSCL 650
1 3UISO- 1HSCL 852
1 RM11-ZERO 1 -642
1 RM22-ZERO 1 -640
1 RM33-ZERO 1 -692
1ABS1- 1ABS2 1000
1 1PF 2-1 1PF 3 -727
v-cov distribution 0...1 by 0.05
430 125 77 34 7 10 7 2 0 1 1 0 2 3 1
0 1 1 0 1
--
Heriot-Watt University is a Scottish charity
registered under charity number SC000278.