Hi All,

I am trying to use the Debye functions in GSAS to look at the amorphous phase in a partially crystallized polymer. I've read the GSAS manual, and see what
the functions are, but cannot figure out how to edit the parameters.

The manual says that the EDTDIFUS subroutine is used for this purpose,
but I can't find that subroutine in the menus in my version of GSAS (Mac OS-X).

Any suggestions would be much appreciated,

David Lee, Ph.D.
SMRL, The Ohio State University
Dept. of Materials Science and Engineering
2041 College Rd
Columbus, OH  43210
(614)-688-3182



Reply via email to