José,

probably this peak is caused by monosulphate - to be more precise by 
calcium aluminium monosulphate hydrate, see PDF no. 44-602). As you 
mentioned the sample to be a "mortar cement", I suppose it is a hydrated 
sample. However, in a mortar I would make sure that the peak is not 
indicating mica or clay minerals, coming from the aggregate.

Best
Christian





José Carlos Cordeiro <[EMAIL PROTECTED]> 
11.07.2008 18:39

To
<[email protected]>
cc

Subject
Identify phases in mortar cement






Someone with expertise in the analysis of hydration cement phases can help 
me to identify the phase with peak in the 8,69 degree in one mortar 
cement, I cannot identify it.
 
regards
 
===========================================
José Carlos Cordeiro
 
DISCLAIMER:
Esta mensagem e seus anexos são destinados exclusivamente ao(s) 
destinatário(s) identificado(s) acima e contêm informações confidenciais 
ou privilegiadas. Se você não é o destinatário destes materiais, não está 
autorizado a utilizá-los para nenhum fim. Solicitamos que você apague a 
mensagem e seus anexos e avise imediatamente o remetente. O conteúdo desta 
mensagem e de seus anexos não representa necessariamente a opinião e a 
intenção da empresa, não implicando em qualquer obrigação ou 
responsabilidade adicionais.
Este mensaje y sus anexos son destinados exclusivamente a los 
destinatarios identificados arriba y contiene información confidencial o 
privilegiada. Si no es el destinatario de este mensaje, o una persona 
autorizada para recibirlo, usted no está autorizada a utilizarlo para 
ningún fin. Cualquier revisión, difusión, distribución o copiado de este 
mensaje está prohibido. Si ha recibido este e-mail por error por favor 
bórrelo y envíe un mensaje al remitente.El contenido de este mensaje y de 
sus anexos no necesariamente representa la opinión o intención de la 
empresa, ni implica ninguna obligación legal o responsabilidad para la 
empresa.
This message and its attachments are addressed exclusively to identified 
addressee and contain confidential and/or privileged information. If you 
are not the addressee or an authorized person to receive this, you must 
not use, copy, disclose or take any action based on this message or any 
information herein. If you have received this message by mistake, please, 
advise the sender immediately by replying the e-mail and delete this 
message. The contents of this message and its attachments do not 
necessarily express the opinion or the intention of the company, and do 
not implies any legal obligation or responsabilities from this company.

"This e-mail is confidential and may contain legally privileged information.
If you are not the intended recipient, you should not copy, distribute, 
disclose or use the information it contains.
Please e-mail the sender immediately and delete this message from your system.
E-mails are susceptible to corruption, interception and unauthorised amendment; 
we do not accept liability for any such changes, or for their consequences.
You should be aware, that the company  may monitor your emails and their 
content"

Reply via email to