Kurt,

 

Back when I was doing this I just purchased Y2O3 from a conventional
chemical supplier and annealed it at high temperature (as high as you
can easily get to, usually something like 1150C unless you have really
fancy furnaces and crucibles) for a few days.

 

Alex Y

 

________________________________________
Dr. Alexandre (Alex) F. T. Yokochi
Assistant Professor
Department of Chemical Engineering
Oregon State University
Corvallis, OR 97331-2702

Voice:  (541) 737-9357
Fax:  (541) 737-4600
http://oregonstate.edu/~yokochia 

        ----- Original Message ----- 

        From: Kurt Leinenweber <mailto:[EMAIL PROTECTED]>  

        To: [email protected] 

        Sent: Tuesday, October 14, 2008 8:17 PM

        Subject: source for Y2O3?

         

        Dear Rietvelders,

         

        In September there was a discussion of refining the polarization
of an instrument, and Lachlan and Matthew both suggested Y2O3.  The time
has come to do the measurement, and I was wondering if anyone has
suggestions for a good source and annealing schedule for the Y2O3?  Is
the already annealed material available as an XRD standard?

         

        Thank you very much,

         

                                                        - Kurt

         

         

        *********

        Kurt Leinenweber

        Dept. of Chemistry and Biochemistry

        Arizona State University

        Tempe, AZ 85287-1604

         

        phone (480)-965-8853

        fax (480)-965-2747

         

        ***********

         

Reply via email to