> The next step would be quantify these phases by Rietveld method using
TOPAS 3.0.
BTW, it shouldn't need a sophisticated Rietveld refinement to distinguish
between the relative quantities of simple FCC and BCC compounds - some
peaks may overlap almost completely, but others not at all.
I worry that people rely so much on databases and computer programmes, and
so little on thinking.
Alan.