Hi Anna,

It is done with the Nsc flag. An example for CW neutron data (Job=1) is
below. The details for other cases are on the pp.79-80 of the manual.

Cheers
Max



-------------------------------------
! Excluded regions (LowT  HighT) for Pattern#  1
        0.00       10.00
      160.00      180.00
! 
! Additional scattering factors for Pattern#  1
B11       0.66500    0.00000   0
!
      19    !Number of refined parameters
!
!  Zero    Code    SyCos    Code   SySin    Code  Lambda     Code MORE
-------------------------------------



-----Original Message-----
From: Anna Llobet [mailto:[email protected]] 
Sent: Thursday, 23 April 2009 7:27 AM
To: [email protected]; Hess, Nancy J
Subject: changing scattering length of element in Fullprof

Can anyone remind me how does one change the scattering length of an 
element when using fullprof?

Thanks

Anna Llobet

-- 
====
Dr. Anna Llobet 
Lujan Neutron Scattering Center
Los Alamos National Laboratory
MSH805
Los Alamos, NM  87545, USA

Phone: +1 505 665-1367     Fax: +1 505 665-2676
Email: [email protected]
http://www.lansce.lanl.gov/
http://www.lansce.lanl.gov/lujan/index.html 
Export license: TSPA, Correspondence 


Reply via email to