Dear Jun Lu,

he is using Rigaku Ultima IV with standard scintillation counter.

With regards,
Eduard.

----- Original Message ----- From: "lu...@ekm" <[email protected]>
To: <[email protected]>
Sent: Saturday, April 25, 2009 3:58 PM
Subject: Re: grazing angle diffraction in single-crystal Si


Dear Levin:

In principle, kinetic scatterring effect can absolutely be avoided by θ-2θ configuration. Did your colleague observe the Si(200) using a special detection setup, image plate for instance? If so, that is really regular.

Faithfully
Jun Lu
----------
Lst. Prof. Lijie Qiao
Department of Materials Physics and Chemistry
University of Science and Technology Beijing
100083 Beijing
P.R. China
http://www.instrument.com.cn/ilog/handsomeland/

Lst. Prof. Loidl and Lunkenheimer
Experimental Physics V
Center for Electronic Correlations and Magnetism (EKM)
University of Augsburg
Universitaetsstr. 2
86159 Augsburg
Germany
http://www.physik.uni-augsburg.de/exp5


Reply via email to