Ross 


The way that I simulate patterns:
I've got a "blank pattern" that has an intensity of 100 counts from 2 to 170 
deg 2theta.
Then I put in the instrument and structure parameters as I see fit, and fix the 
scale factor in the structure(s); et voila! A simulated pattern :)




Cheers

Matthew

________________
Matthew Rowles

CSIRO Minerals
Box 312
Clayton South, Victoria
AUSTRALIA 3169

Ph: +61 3 9545 8892
Fax: +61 3 9562 8919 (site)
Email: [email protected]
-----Original Message-----
From: Ross H Colman [mailto:[email protected]] 
Sent: Monday, 6 July 2009 20:36
To: [email protected]
Subject: Dummy pattern within TOPAS

Dear Rietvelders,

I am looking to generate a number of 'dummy' powder neutron diffraction
patterns within TOPAS for comparison purposes. I know that this can be
done within Fulprof using the Job=3 mode but could not find anything
within the TOPAS manual/examples about generation of simulated patterns.

If it is possible could someone send me the command/macro or an example of
its use in an INP file?

Thank you in advance for any help you may have.
Best regards
Ross Colman