Dear Angel,

I think you should pay attention to articles by Paolo Scardi and Matteo Leoni. They have developed a very powerful technique called WPPM (Whole Powder Pattern Modelling) which is designed for microstructural analysis from XRD data.
I suggest that you should check these papers:

1. P. Scardi, M. Leoni. Acta Cryst A58 (2002) 190-200.
2. M. D'Incau, M. Leoni, P. Scardi. J. Mater. Res. 22 (2007) 1744-1753
3. J. Martinez-Garcia, M. Leoni, P. Scardi. Acta Cryst A65 (2009) 109-119

and references therein.

A short and simple answer will be that XRD profiles taken for ball-milled materials are much more distorted by dislocations than by vacancies. One of the simple reasons is that dislocation-induced strain field decays as 1/R and vacancies-induced strain field decays as 1/R^2 where R is distance from diclocation core or vacansy center.

With best regards,
Eduard.

----- Original Message ----- From: "Angel L. Ortiz" <[email protected]>
To: <[email protected]>
Sent: Wednesday, September 09, 2009 11:32 AM
Subject: defect measurement


Dear colleagues:



I am writing to formulate a question on the evaluation of defects by XRD.
This is the following:



I have a ball-milled material, and I would like to define the type of
defects induced by the ball milling. In particular, I would like to
elucidate whether the ball milling has induced vacancies, or dislocations.



Could any of you help in this issue, and indicate how this can be done and
how one can know the type of defect from the XRD pattern?



Thanks a lot,



Angel