Dear Nelson,
you probably could use LaB6 or you could buy an alpha-corundum fron Alfa
Aesar, it's very cheap and will give you good results.
At the end, you should select an internal standad with x-ray absorption
coefficient similar to your sample, but you can correct this effect with
any software.
If anyone can correct me, please feel free to do it, because I'm new at
diffraction world.
Cheers,
Cristóbal
El 04/09/2013 15:59, led15 escribió:
Dear colleagues,
could anybody suggest a standard (and where i can buy), not very
expensive, like quartz or zirconia to doping a power sample to
control the position of xrd lines and probably later help in
quantification.
we use Nist standard LaB6 to instrument performance characterization
Thanks a lot.
Nelson
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++