John is correct, be careful that you are trying to compare same quantities but
in a completely different units and definitions. I discover by myself that you
cannot mix scattering factors, absorption factors, photo absorption etc. coming
some from the diffraction community and some from the spectroscopic community.
So Henke is used by the spectroscopic community (second link) and need proper
conversion to be applied for scattering…..
I actually use Henke derived work in Maud now as I can compute the dispersion
coefficients (and absorption) for every wavelength not only the tabulated ones
usually adopted in diffraction, but I had to convert everything to be
consistent (absorption etc.).
Best regards,
Luca
> On Jun 11, 2015, at 6:07 PM, Jonathan WRIGHT <[email protected]> wrote:
>
> Dear Xiaodong, Jeremy,
>
> Isn't it equation 3 here?
> http://www.nist.gov/srd/upload/jpcrd488.pdf
> <http://www.nist.gov/srd/upload/jpcrd488.pdf>
> f1/f2 are "dispersion" numbers and f'/f" are the "anomalous" ones. The
> relativisitic correction number for iron then shows up on page 221.
>
> Best,
>
> Jon
> ===
>
> On 11/06/2015 17:27, Jeremy Karl Cockcroft wrote:
>> Hi Xiaodong,
>> I think that the numbers quoted for f' in the second case have had 26e
>> (atomic no.) added to them, i.e. it refers to the total dispersion value for
>> the real component (as opposed to the imaginary component). Given that the
>> numbers quoted are close to an absorption edge, then the remaining
>> differences are not unexpected depending on source and precise energy
>> quoted. If graphs of the data are plotted with Z subtracted, then they look
>> very similar apart from the precise value of the minimum of f' at the
>> absorption edge itself.
>> Just my thoughts on it...
>> Jeremy Karl.
>> ***************************************************************
>> Dr Jeremy Karl Cockcroft
>> Department of Chemistry
>> (University College London)
>> Christopher Ingold Laboratories
>> 20 Gordon Street
>> London WC1H 0AJ
>> United Kingdom
>> +44 (0) 20 7679 1004 (laboratory)
>> [email protected] <mailto:[email protected]> or
>> [email protected] <mailto:[email protected]>
>> http://img.chem.ucl.ac.uk/www/cockcroft/homepage.htm
>> <http://img.chem.ucl.ac.uk/www/cockcroft/homepage.htm>
>> ***************************************************************
>>
>>
>> On 11 June 2015 at 15:33, iangie <[email protected] <mailto:[email protected]>>
>> wrote:
>> Dear Rietvelders,
>>
>> I am little confused about the term "Anomalous scattering factor" and
>> "Dispersion coefficients".
>> "Anomalous scattering factor" can be found here
>> http://skuld.bmsc.washington.edu/scatter/AS_form.html
>> <http://skuld.bmsc.washington.edu/scatter/AS_form.html>
>> "Dispersion coefficients" can be found here
>> http://www.cxro.lbl.gov/optical_constants/asf.html
>> <http://www.cxro.lbl.gov/optical_constants/asf.html>
>>
>> Their numbers are quite different: e.g. Fe @ CrKα: f0=18.474, Δf'=-1.6
>> Δf"=0.9 ; however, the corresponding dispersion coefficients are f'
>> ~24.6808 and f" ~0.759346
>> Can anyone explain their relationship?
>>
>> Thanks!
>> --
>> Yours Sincerely,
>> Dr. Xiaodong(Tony) Wang
>> XRD Application Scientist
>> Bruker Singapore Pte. Ltd.
>>
>> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
>> Please do NOT attach files to the whole list <[email protected]>
>> <mailto:[email protected]>
>> Send commands to <[email protected] <mailto:[email protected]>> eg: HELP as the
>> subject with no body text
>> The Rietveld_L list archive is on
>> http://www.mail-archive.com/[email protected]/
>> <http://www.mail-archive.com/[email protected]/>
>> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
>>
>>
>>
>
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
> Please do NOT attach files to the whole list <[email protected]>
> Send commands to <[email protected]> eg: HELP as the subject with no body text
> The Rietveld_L list archive is on
> http://www.mail-archive.com/[email protected]/
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
>
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++