Dear Alan,

I have a few patterns of samples in 0.3mm Boron-Rich Glass capillaries but 
collected in Debye-Scherrer mode.
What does "Capillary Specimen data collected in reflection mode" mean, high 
angle peaks only?


Cheers!

--

Yours Sincerely,
Dr. Xiaodong(Tony) Wang
XRD Application Scientist
Bruker Singapore Pte. Ltd.


At 2015-06-15 00:32:03, "Alan Coelho" <[email protected]> wrote:


Hi all

 

I'm looking  for Capillary Specimen data collected in reflection mode which 
shows odd bumps on the peaks. I'm aware that there are supposed to be odd 
shaped peaks but I am looking for example data that show it. If anyone has such 
data and are willing to part with it then let me know.

cheers
alan
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++