Julian,

First, the best idea would be to use a NIST standard to qualify your secondary 
standard. With this in mind, you can use almost any secondary standard. Since 
you have a silica matrix you probably want to use corundum powder since the 
absorption is similar.

Have you considered using an external standard method? The advantages are:

1.       No mixing errors (inhomogeneity)

2.       The original sample is not diluted

3.       No peak overlap between standard and sample

4.       The mass absorption coefficient of the standard doesn't need to match 
the sample.

The method works very well for complicated mixtures with many phases. The 
disadvantage is that it may be more complicated to setup the method initially.

The original method is described here:
O'Connor and Raven, Application of the Rietveld refinement procedure in 
assaying powdered mixtures, Powder Diffraction Vol. 3/1, 2-6, 1988

A more practical solution by example of cement is given here:
Jansen et al, Does Ordinary Portland Cement contain amorphous phase? A 
quantitative study using an external standard method, Powder Diffraction Vol. 
26/1, 31-38, 2011

A comparison is given here. In my opinion, the choice of test samples is not 
favorable to the external standard method.
Madsen et al, Description and survey of methodologies for the determination of 
amorphous content via X-ray powder diffraction, Zeitschrift für 
Kristallographie Volume 226, Issue 12 (Dec 2011)


Best regards,
Jeff

Jeffrey Nicolich  | Principal Scientist
Grace, 62 Whittemore Ave, Cambridge, MA, 02140, USA  |  T +1 617.498.3816
[email protected]<mailto:[email protected]>
________________________________
THIS E-MAIL AND ANY ATTACHED FILES ARE CONFIDENTIAL AND MAY BE LEGALLY 
PRIVILEGED. If you are not the addressee, any disclosure, reproduction, 
copying, distribution, or use of this communication is strictly prohibited. If 
you have received this transmission in error please notify the sender 
immediately and then delete this e-mail.

From: [email protected]<mailto:[email protected]> 
[mailto:[email protected]] On Behalf Of Julian Richard Tolchard
Sent: Thursday, October 08, 2015 1:28 PM
To: [email protected]<mailto:[email protected]>
Subject: Quantitative internal standards

Hi all,

I've been asked to do some quantification on some samples which are 
predominantly silica, which means a reasonable amorphous component is pretty 
much inevitable. I'm thus looking for a suitable internal standard for spiking, 
but as this could be quite a big project moving forwards i don't think the NIST 
standards are financially viable. Does anyone have any good sources for spikes 
to use with such light materials?

Regards,


jools

++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to