Hi Francois,

We use the Leister LE mini heat gun pretty routinely for temperatures up to 600 
C with Bruker D8 capillary set ups. We use Leister's own control box (which you 
need to put into "advanced user" mode to control ramp rates etc), which is fine 
for most things. It should also be possible to control the LE Mini with 
something like a Eurotherm programmable controller which could interface with 
your data collection software.

We also have the excellent Anton Paar HTK1200 chamber with a capillary adapter, 
for going up to 1000 C, but this is probably a bit overkill for your 
application.

Best regards,

Dave


Dr David Wragg
Laboratory Manager
Norwegian National Centre for X-ray Diffraction and Scattering
University of Oslo
0315 Oslo
Norway

Tel. +47 22858232

________________________________________
From: [email protected] <[email protected]> on behalf of 
François Goutenoire <[email protected]>
Sent: 01 March 2017 12:13
To: [email protected]
Subject: heater system in transmission

Dear Rietveld users,

We would like to buy or to built an heater system for our laboratory
system (Empyrean equipped in transmission with capillary). The aim is to
reach 200-300°C, this is mainly for organic compounds. I have few
questions : if we use an air blower is there any problem for the
goniometer ? In comparison with air blower found in large instrument
(ESRF, …..)

Does anyone has constructed is own system (infrared heating system ?
External Kapton shield ?...)

Thank in advance for the answers and discussions

François

--
*********************************************************************************************
Pr. Francois GOUTENOIRE
e-mail: [email protected]
Tel: 02.43.83.33.54
FAX: 02.43.83.35.06
Département des Oxydes et Fluorures
Institut des Molécules et des Matériaux du Mans
IMMM - UMR CNRS 6283
Université du Maine - Avenue Olivier Messiaen
F-72085 Le Mans Cedex 9
FRANCE
*********************************************************************************************
Formation Rietveld CNRS
https://cnrsformation.cnrs.fr/stage.php?stage=17082
Formation SASX CNRS
https://cnrsformation.cnrs.fr/stage.php?stage=17228


---
L'absence de virus dans ce courrier électronique a été vérifiée par le logiciel 
antivirus Avast.
https://www.avast.com/antivirus

++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to