This is one of many types of diffraction questions that can be effectively addressed by carrying out simulations in your favorite software for Rietveld refinement. Fix all other parameters and vary the preferred orientation parameters, and you will get your answer.
Regarding Alan’s answer, you may wish to think about the difference between a Si powder standard sample and a zero-background Si holder. Professor Chemist Dept. of Chemistry Dept. of Chemistry Stony Brook University Brookhaven National Laboratory Stony Brook, NY 11794-3400 Upton, NY 11973-5000 Office: 447 Grad. Chemistry Office: Bldg 555, Rm 340 Phone: (631)632-7796 Phone: (631)344-7689 Fax: (631)632-7960 Fax: (631)344-5815 Web page: https://sites.google.com/a/stonybrook.edu/pgk/home<https://urldefense.proofpoint.com/v2/url?u=https-3A__sites.google.com_a_stonybrook.edu_pgk_home&d=DwMFaQ&c=aTOVZmpUfPKZuaG9NO7J7Mh6imZbfhL47t9CpZ-pCOw&r=BX8us55AyPAIC_WBilHRkA&m=Ct0KZCwEwpWRcA5CUercOpxFrSByRm-qocG1lq-PEZc&s=joWXazAAemA3JtxXYrqXryS48Uko6JW70pfW7PzQSWc&e=> From: [email protected] <[email protected]> On Behalf Of Shay Tirosh Sent: Wednesday, April 22, 2020 8:18 AM To: [email protected] Subject: Integrated intensities issue. Dear Rietvelders I hope you all feeling well and surviving the Coronavirus. Does the integrated intensity corresponding to a reflection peaks of oriented material and randomly oriented are the same? Please note in bough case the volume fraction of the material is the same, Only the orientation is not. Thanks Shay -- _________________________________________________ Dr. Shay Tirosh Institute for Nanotechnology & Advanced Materials Bar Ilan University Ramat Gan, 52900 Israel Phone: +972-(0)30-531-7320 Mobile: +972-(0)54-8834533 Email: [email protected]<mailto:[email protected]> _________________________________________________
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++ Please do NOT attach files to the whole list <[email protected]> Send commands to <[email protected]> eg: HELP as the subject with no body text The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/ ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++