Dear Rietveld users,

We are currently looking for the atomic structure (cif file) of the C60 Orthorhombic cell

The previous paper : "Structure and superconductivity of single crystalline C60" from Koichi Kikuchi et al.

Physica C in 1975

The cell parameters are given  a=25.011 Ang, b=25.582 Ang. c=10.003 Ang. Space group Pbnm

but there is not atomic position in the paper.

Best regards, françois Goutenoire

--
*********************************************************************************************
Pr. Francois GOUTENOIRE
e-mail: [email protected]
Tel: 02.43.83.33.54
FAX: 02.43.83.35.06
Skype Entreprise visio conférence
Département des Oxydes et Fluorures
Institut des Molécules et des Matériaux du Mans
IMMM - UMR CNRS 6283
Université du Maine - Avenue Olivier Messiaen
F-72085 Le Mans Cedex 9
FRANCE
*********************************************************************************************
Formation Rietveld CNRS 2020
https://cnrsformation.cnrs.fr/diffraction-des-rayons-x-sur-materiaux-polycristallins?axe=135
Formation EDX CNRS 2020
https://cnrsformation.cnrs.fr/fluorescence-x-edx?axe=135
Formation SAXS et Réflectivités pour couches minces et matériaux nanostructurés.
https://cnrsformation.cnrs.fr/caracterisation-des-materiaux-nanostructures-par-diffusion-des-rayons-x?axe=135
Bibliographie
https://scholar.google.fr/citations?hl=fr&user=qC-lmN4AAAAJ&view_op=list_works&authuser=1&sortby=title
https://orcid.org/0000-0001-5339-3002

++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to