Dear François,

The easy way we have found to do that is by isolating the open aperture
with vacuum grease inside the glove box and theb taking them outside where
you can seal them easily with a lighter.

Hope it helps

Best,

Le lun. 30 janv. 2023 à 12:01, francois Goutenoire <
francois.gouteno...@univ-lemans.fr> a écrit :

> Dear Rietveld users,
>
> We are currently working with some very hygroscopic compounds in
> capillaries.
>
> These capillaries are fill in a glove box (N2).
>
> How can we sealed these capillaries (borosilicate) in the glove box ?
>
> Best wishes, François
>
> --
> *********************************************************************************************
> Pr. Francois GOUTENOIRE
> e-mail: francois.gouteno...@univ-lemans.fr
> Tel: 02.43.83.33.54
> FAX: 02.43.83.35.06
> Institut des Molécules et des Matériaux du Mans
> IMMM - UMR CNRS 6283
> Elaboration et Caracterisation des Composés Cristalisés (E3C)
> Université du Maine - Avenue Olivier Messiaen
> F-72085 Le Mans Cedex 9
> FRANCE
> *********************************************************************************************
> Formation Rietveld 
> CNRShttps://cnrsformation.cnrs.fr/diffraction-des-rayons-x-sur-materiaux-polycristallins?axe=135
> Formation EDX CNRShttps://cnrsformation.cnrs.fr/fluorescence-x-edx?axe=135
> Formation SAXS et Réflectivités pour couches minces et matériaux 
> nanostructurés.https://cnrsformation.cnrs.fr/caracterisation-des-materiaux-nanostructures-par-diffusion-des-rayons-x?axe=135
> Bibliographiehttps://scholar.google.fr/citations?hl=fr&user=qC-lmN4AAAAJ&view_op=list_works&authuser=1&sortby=titlehttps://orcid.org/0000-0001-5339-3002
>
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
> Please do NOT attach files to the whole list <alan.he...@neutronoptics.com
> >
> Send commands to <lists...@ill.fr> eg: HELP as the subject with no body
> text
> The Rietveld_L list archive is on
> http://www.mail-archive.com/rietveld_l@ill.fr/
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
>
>
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to