Il 13/11/2023 18:35, Claire Emily Boronski ha scritto:

Dear Claire,

Make the sum of the remaining crystalline weight percentages to be 100%. This is a rough, but simple, calculation. Alternatively, measure an empty capillary and correct the raw data of your mixture for such scattering (taking into account by X-ray tracing the effect of filling the capillary by an absorbing material).
Norberto

        
Some people who received this message don't often get email from [email protected]. Learn why this is important <https://aka.ms/LearnAboutSenderIdentification>
        

Hi All,

I am trying to exclude the glass capillary from the weight percent calculations in my Rietveld refinement. I modeled the glass capillary using a SiO2 CIF file and made the crystallite size very small. The issue I am having now is that in the weight percent calculation it is saying the glass is ~90% of the weight. Does anyone know how I can exclude this phase from the weight percent calculation?

Thanks,

Claire


++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list<[email protected]>
Send commands to<[email protected]>  eg: HELP as the subject with no body text
The Rietveld_L list archive is onhttp://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++


--
Norberto Masciocchi
Professor of Chemistry
Department of Science and High Technology & To.Sca.Lab.
University of Insubria
Via Valleggio, 11
22100 Como - Italy
E-mail:[email protected] Tel: +39-031-2386613
Skype: norberto.masciocchi
Website: toscalab.uninsubria.it
******************************************
Hago cosas que me quitan un poco el mal gusto del vacío.
Y ésa es en el fondo la mejor definición del homo sapiens (J. Cortàzar)
******************************************
Justice is nothing more than the advantage of the stronger (Thrasymachus)
******************************************
Freedom is just another word for nothing is left to lose (K. Kristofferson)
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to