Re: Rietveld refinement in TOPAS with parallel beam geometry

2009-12-04 Thread Patrick Price
Patrick, > > > From: Patrick Price [patrickpric...@gmail.com] > Sent: Friday, December 04, 2009 6:30 AM > To: Rietveld_l@ill.fr > Subject: Rietveld refinement in TOPAS with parallel beam geometry > > Since this is my first post I will start with a brief introduct

Rietveld refinement in TOPAS with parallel beam geometry

2009-12-04 Thread Patrick Price
Since this is my first post I will start with a brief introduction. My name is Patrick Price and I am in my second year of graduate school. My thesis work involves the investigation of phase equilibria in perovskites. I am using a Bruker D8 Discover diffractometer with parallel beam geometry. The