Dear Rietvelders,
I am using Fullprof to microstructural analysis of particles. I have
one type of particle but different sample with different sizes
(particles increase after heat treatment). Their crystallites size
fluctuates between 10nm and 1µm. I know that 1µm is big for a refinement
Ri