At 19:26 08/02/2001, you wrote:
someone could give me the structure of silicon carbide 6H ? please?
From ICSD (look for Moissanite, there are 41 entries):
Shaffer,PTB. (1969) Acta Crystallogr.,Sect. 25 477-488
A review of the structure of silicon carbide
GomesdeMesquita,AH. (1967) Acta
On 20/11/2000, Armel wrote in answer to Daniela Kovacheva, who wrote:
Could somebody send me information about the structure of Ni2GeS4?
This is typically a case for which you need several databases
for solving it. Nothing about Ni2GeS4 in ICSD nor in CRYSTMET...
The ICDD JCPDS database says