Hi Antonio
I have tried the position of C atom, and i have supposed that could be in
8a,whic is an intersticial position, as Frank says, but you have to
specify the site occupation, which is related to carbon content.
Best wishes.
Miguel Hesiquio
On Fri, October 31, 2008 8:05 am, Frank
Hi to all!,
in fact, the Cagliti's expression is just a way to show the angular
variation of fwhm, as was mentioned was usef for neutron diffraction and
adopted in XRD, we can also build another dependence such as FWMH vs
2theta directly and it is useful to evaluate size and strain, the problem