These are quotes from Action Electronics silver maker.

Why did they stop recommending salt?  "We have been told that this method
is becoming the preferred method.  It produces a high quality colloid of
even smaller particles and helps ensure an even longer shelf life for
storage."

How many ppm will you get?  "Leave on for 10 minutes per 8 oz. will produce
a solution of approximately 5 parts per million.  You will not see a white
haze coming off the electrode as you did if you had previously used the
salt solution."

They have you make 8 oz. to start with and divide that into 2 oz.
proportions and make 4 batches from it.  A batch would consist of 2 oz. of
starter (old silver mixture) and 6 oz. of hot distilled water.  

I'm new at this, but between what I learned from my instructions and things
I've learned from the list, this is what I'm doing.  I'm making 1 1/2
quarts (48 oz) at a time.  Happens to be the size of the glass pot I
bought.  I use 12 oz. of starter and 36 oz distilled water. I bring it to
the boiling point.   I also leave my batch on the stove on low to keep it
warm.  I leave it on for about l 1/2 to 2 hours.  This is only the 3rd
batch I've made.  This last batch has a beautiful golden yellow color.

I was just thinking that maybe I shouldn't be bringing my starter to boil
with the distilled water.  It may alter it. 

Margaret 


----------
> From: M. G. Devour <[email protected]>
> To: [email protected]
> Subject: Re: salt/no salt
> Date: Saturday, January 10, 1998 4:43 AM
> 
> Hey gang!
> 
> The 64 thousand dollar question is...
> 
> Now that Beck and others have dropped the salt, how long do they tell 
> you to run the process, and how many ppm do they say you'll get?
> 
> Mike
> 
> [Mike Devour, Citizen, Patriot, Libertarian]
> [[email protected]                       ]
> [Speaking only for myself...              ]