>From the Hanna literature I take it that a four probe system is employed. Two probes across from each other pass a known current. The other two sense the flow and amplify. The temperature is measured and taking into account. Of course the silver is not dissolved at all but is only hanging out in the water molecule. The oxygen would be as a house, the hydrogen as a dog, and the bitty little silver from a single atom to atom clusters of silver. These are suspended by like repulsion either positive or negitive so I guess the TDS does not give a measure of true ppm of a sol, but it is still quantitative.
On Thu, 10 Jun 1999 20:58:24 -0400, Marshall Dudley wrote: > How is the measurement made? If it is by resistance I can believe the > reading, that is I would expect them, but they would be wrong as far a ppm is > concerned. > Marshall > Scharbach wrote: >> A higher ppm on a 2 hour batch of silver than on a 12 hour batch? >> DId you do something else different? >> Sparrow >> >My tds1 came today and after calibrating checked out my CS. >> > >> >HVAC 2 hour batch - 26 ppm. clear, light tyndall >> >HVAC drip 2 minute batch 3 ppm. clear, very light tyndall >> >LVDC 12 hour batch 6 ppm, yellow, very strong tyndall >> >LVDC 2 hour batch, 12 ppm clear, good (distinct) tyndall >> > >> >If I remember right the folks who use these to monitor their production >> >figure the CS ppm as 1/2 the tds1 meter reading? This has been verified >> >by other testing if memory serves. >> > >> >Please clarify if possible. Thanks...RONjb -- The silver-list is a moderated forum for discussion of colloidal silver. To join or quit silver-list or silver-digest send an e-mail message to: [email protected] -or- [email protected] with the word subscribe or unsubscribe in the SUBJECT line. To post, address your message to: [email protected] List maintainer: Mike Devour <[email protected]>