To the New CS makers,

I've been making CS for 10 months, a couple batches
a week. Using steam distilled water is THE MOST IMPORTANT 
part of generating a successful batch of CS.

Takes me about an hour to make 20 ounces. Less time if a 
tablespoon of previously made CS is added. Never saw the
benefit to heating the water, so no inputs on that subject.

For the seasoned CS makers:
Monitoring and limiting run current to 1 milli-amp made a 
BIG difference in consistency and quality batch to batch. 
Run time increases to about 2 hours though.
I almost always get clear CS with good Tyndall effect.

Stay healthy,
Tom Bassett




--