Wow- that is one cool picture. Do you add h2o2 to every batch? I only add it when it is turning color. Maybe I could add it everytime.

On Nov 7, 2007, at 6:17 AM, Ode Coyote wrote:

I find that around 6 drops of 3% to the quart added at least 2 or 3 days after the batch is done, does the job.
 It can take several hours, even days, to complete that job.
Add a drop to a sample. If it shows a fast reaction [white or brown murky], wait longer.

 Micrographs thanks to Nancy Delese
[This is what mostly ionic silver actually looks like under a very strong microscope, not that dark field of specks that a TEM photo shows....which is 97% oxidized ions, not " the particles", at all ]
http://silverpuppy.com/csh2o2.html

ode


At 09:54 PM 11/6/2007 +0100, you wrote:
>So would you say that EIS with H2O2 added is safe to use as you would use EIS with nothing added?
If so, how much H2O2 should be added and when should it be added?

Thank you.
Ian


--
The Silver List is a moderated forum for discussing Colloidal Silver.

Instructions for unsubscribing are posted at: http://silverlist.org

To post, address your message to: [email protected]

Address Off-Topic messages to: [email protected]

The Silver List and Off Topic List archives are currently down...

List maintainer: Mike Devour <[email protected]>