James said:
Hi Fred,
Will you provide your reasoning and data for the statement:
"HVAC produces an inferior product - non-ionic and non-colloidal.
(although possibly better for topical uses due to the high PPM
possible!)"?
Reply - Per my previous post, HVAC will first release an ion of silver,
from the positive electrode - then the voltage reverses and it will be
attracted right back to the now negative electrode and gain its electron
which converts it to elemental silver (every bodies 'sludge'). The heavy
fluid circulation from the HV electrostatic forces blows it into the water!
Now, this is a not a colloid or solution but a 'suspension' of very tiny silver
particles with no charge. Thus, non-ionic and non-colloidal. I believe we
all agree on the higher bio-availability and effectiveness of ionic and
colloidal minerals!
James said:
Also, I am very interested in how to obtain high PPM HVAC sol. What do you
call "high" PPM.
Fred replied:
The practical limit for an ionic colloid of silver seems to be around 25 PPM
as we start forming crystals around that level. (People who do not circulate
their "cloud of ions" will have much higher levels in the cloud and thus the
propensity to form crystals and shorter shelf life.) The HVAC 'suspension'
should
have a much higher limit of PPM (up to a sautration level) as there is no
crystal
growth below a saturation level when no electric charges are present. I see
ads for 50-500 PPM and expect they are possible. Taking high PPM will of
course introduce an opportunity to overdose (blue), which I do not believe is
possible with a true 5PPM colloid.
James said:
The LV stuff I used to make was effective, but had only about a 30 day life
before a large amount of it fell out. I presume its particle size was
rapidly increasing, and available silver was decreasing. This does not
happen with the HV sol. Nor has any of it ever changed color if clear when
made.
Fred replied - Short shelf life is an indication of crystals settling by
gravity!
They would not normally grow unless ions of silver were also present.
The PPM is the same (by weight) but the TDS would fall off! The HVAC product
should have minimal sized particles, no charge so no crystal growth and thus
a long fallout time.
James said:
Regarding cone formation, could you give a little more detail about the
"...very powerful electrostatic forces."?
Would you explain the relationship between 60 Hz and "static"?
Fred replied - It is the electrostatic force that lifts the mass of water up to
the top electrode (above the water surface). Electrostatic forces, like magnetic
can be appreciable. The electrostatic energy imparted to an ion is measured
in electron-volts and having 10,000 volts helps a lot. 60HZ is of course
alternating from positive to negative at each electrode, letting each charged
particle take electric energy and give it up 60 times a second, while with DC
(static) the polarity is fixed and a charge is taken and maybe minutes later
given
up, but only if it ever reaches the other electrode or a crystallization site.
Cordially, [email protected]
--
The silver-list is a moderated forum for discussion of colloidal silver.
To join or quit silver-list or silver-digest send an e-mail message to:
[email protected] -or- [email protected]
with the word subscribe or unsubscribe in the SUBJECT line.
To post, address your message to: [email protected]
Silver-list archive: http://escribe.com/health/thesilverlist/index.html
List maintainer: Mike Devour <[email protected]>