Greetings Seekers;
Ivan, our numbers are similar (.59 to .57) but I think you may have them
backwards. The instructions from Hanna and what my lab results confirmed was
.59PPM/us. or take the reading in us/cm times .59 to get PPM. In my case
25.5us/cm = 15 PPM. per lab test. Also the us/cm will drop with time for the
first 10-12 hrs, not rise. This appears to be due to the CS dispersing
throughout the DW. Immediately after making a batch the CS is concentrated
around the ion path between the electrodes. A reading taken at this time will
be high and erratic. After sitting overnite the reading will be lower but
stabile. After this initial dispersion the reading should not change futher. I
have CS that is now several months old that still reads within 1 us/cm of when
it was made. As for accuracy my PWT measures in .1us/cm up to 99.9us/cm. I
calibrate it using a solution from Hanna that measures 84us. It comes in small
pouches that you tear open and insert the meter. Use once and throw away.
NAMASTE'
Beldohr

____________________________________________________________________
Get your own FREE, personal Netscape WebMail account today at 
http://webmail.netscape.com.


--
The silver-list is a moderated forum for discussion of colloidal silver.

To join or quit silver-list or silver-digest send an e-mail message to: 
[email protected]  -or-  [email protected]
with the word subscribe or unsubscribe in the SUBJECT line.

To post, address your message to: [email protected]
Silver-list archive: http://escribe.com/health/thesilverlist/index.html
List maintainer: Mike Devour <[email protected]>