Right Marshall, That's probably the difference between Ol' Bob's and my experiments too...I have an awful lot of area of silver 8300 square mm immersed in the 4KVDC unit .
At any single point on the electrode surface the current would be quite low, allowing the total current carried in the batch to still be fairly high. That explains the quick batching and water warming, and the stability of the batch. It also explains a bit about why I have to stop and stir it every 35 to 45 seconds. I've got to get a low-volume pump and make continuous batches so I don't have to stir. Unlike Bob's latest 6KV pulsed batch that shows sparkles, mine has a low tyndall effect and no sparkes at all. Perhaps the power ratio to electrode size is important WRT DC generation. I've been giving some thought to selling some so I could experiment more, but I'm reluctant to stop giving it away. Thanks for your help. ----- Original Message ----- From: Marshall Dudley <snip>I suspect the difference is that for LV a large electode area is used, giving a fairly linear voltage gradient from one electrode to the other,</snip> ciao Duncan -- The silver-list is a moderated forum for discussion of colloidal silver. To join or quit silver-list or silver-digest send an e-mail message to: [email protected] -or- [email protected] with the word subscribe or unsubscribe in the SUBJECT line. To post, address your message to: [email protected] Silver-list archive: http://escribe.com/health/thesilverlist/index.html List maintainer: Mike Devour <[email protected]>