Greetings EIS'ers, As Mike has noted the DW has changed. At KC MO in the past the DW was made at Hazelwood MO, it is now made at KC Kansas.
The Hazelwood DW ususally had a Cf of 2.0 to2.5 uS/cm. The KC Kansas DW runs about 4.0 to 5.0 uS/cm. But that does not account for the shape of the data that I have plotted for both. Every batch I make has the cell current, voltage, and conductance recorded. for those who have Wplot16.exe or Wplot32.exe look at the shape of the current curves. they are entirely different. as is the conductance curve. Any answers??? "Ole Bob"
5x8 Anode 4Cm.PLT
Description: application/unknown-content-type-plt_auto_file
AWMKSA.PLT
Description: application/unknown-content-type-plt_auto_file
AWMKSB.PLT
Description: application/unknown-content-type-plt_auto_file