Bill,

I use Pro Set and it has all the post curing information right on it. Its a two phase curing process and I don't remember exactly what the times are, but I seem to remember 105 degrees for 24 hours. It does depend on the brand and "model".

As far as I remember, West Systems doesn't really benefit from a post cure under heat.

Have fun/Anker

Anker

Bill & Bunny Kuhlman wrote:

Granddaughter Alyssa and I are involved in vacuum bagging processes: carbon fiber spar caps, fiberglass over foam flying surfaces, and a molded all glass fuselage pod and boom.

We're using West System 105/206 for all of the components.

We know that post curing - higher than room temperature heat over several hours to a full day - will make the epoxy matrix stronger, but after a long web search have been unable to get firm numbers for either the temperature required or the recommended time period.

If anyone can pass on this information, we'd very much appreciate it. We have our "hot box" made and can take it up to 160 degrees F.

Many thanks in advance!

RCSE-List facilities provided by Model Airplane News.  Send "subscribe" and 
"unsubscribe" requests to [EMAIL PROTECTED]  Please note that subscribe and unsubscribe 
messages must be sent in text only format with MIME turned off.  Email sent from web based email 
such as Hotmail and AOL are generally NOT in text format