In message <[email protected]>, Andreas Bergmann 
writes:
>Hello David,
>
>On 01.11.2016 15:50, David wrote:
>> avoid Mylar/polyester/PET and high dielectric constant ceramic
>> capacitors.
>
>Do you have some specific recommendations/suggestions what to use?
>
>Polypropylene? PTFE? Wet Tantalum capacitors (extreme expensive)?

Mica or Teflon


-- 
Poul-Henning Kamp       | UNIX since Zilog Zeus 3.20
[email protected]         | TCP/IP since RFC 956
FreeBSD committer       | BSD since 4.3-tahoe    
Never attribute to malice what can adequately be explained by incompetence.