Hi all, The new NIST SRM for analysis of crystallite size that I have spoken about on a number of occasions over the years is now available. SRM 1979 - Powder Diffraction Line Profile Standard for Crystallite Size Analysis (Nano-Crystalline ZnO Powder) https://www-s.nist.gov/srmors/view_detail.cfm?srm=1979 Regards, Jim
James P. Cline Materials Measurement Science Division National Institute of Standards and Technology 100 Bureau Dr. stop 8520 [ B113 / Bldg 217 ] Gaithersburg, MD 20899-8523 USA jcl...@nist.gov<mailto:jcl...@nist.gov> (301) 975 5793 FAX (301) 975 5334
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++ Please do NOT attach files to the whole list <alan.he...@neutronoptics.com> Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/ ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++