RE: Mixed refinement Topas example

2018-11-02 Thread Cline, James Dr. (Fed)
François,

Somewhat more than slightly curious: Why do you want to use Topas in GUI mode?

Jim


James P. Cline
Materials Measurement Science Division  
National Institute of Standards and Technology
100 Bureau Dr. stop 8520 [ B113 / Bldg 217 ]
Gaithersburg, MD 20899-8523    USA
james.cl...@nist.gov
(301) 975 5793

-Original Message-
From: rietveld_l-requ...@ill.fr  On Behalf Of Luzia 
Germann
Sent: Friday, November 02, 2018 9:17 AM
To: rietveld_l@ill.fr
Subject: Re: Mixed refinement Topas example

Hey François,

You can find an example (with input file) on John's wonderful webpage under the 
following page:

https://na01.safelinks.protection.outlook.com/?url=http%3A%2F%2Fcommunity.dur.ac.uk%2Fjohn.evans%2Ftopas_workshop%2Ftutorial_combined.htmdata=02%7C01%7Cjames.cline%40nist.gov%7Cb56878acaf134a6fdd5a08d640c58634%7C2ab5d82fd8fa4797a93e054655c61dec%7C1%7C0%7C636767614451670425sdata=Yhn2S6ldVw2lvbtDMOTT%2Fza6gjO0I73iBncJDpdM1tw%3Dreserved=0

There are also other, really cool tutorials, worth checking out!

Best,
Luzia

Quoting François Goutenoire :

> Dear Rietveld users,
>
> I am starting with Topas5.0 commercial, and I would like to do a mixed 
> X-Ray-Neutron refinement directly on GUI mode.
>
> Does anyone can send me an example of *.PRO file or even an *.INP file 
> to to the refinement in launch mode.
>
> The neutron data are with constant wavelength.
>
> Thanks in advance.
>
> --
> **
> ***
> Pr. Francois GOUTENOIRE
> e-mail: francois.gouteno...@univ-lemans.fr
> Tel: 02.43.83.33.54
> FAX: 02.43.83.35.06
> Skype Entreprise visio conférence
> Département des Oxydes et Fluorures
> Institut des Molécules et des Matériaux du Mans IMMM - UMR CNRS 6283 
> Université du Maine - Avenue Olivier Messiaen
> F-72085 Le Mans Cedex 9
> FRANCE
> **
> ***
> Formation Rietveld CNRS 2019
> https://na01.safelinks.protection.outlook.com/?url=https%3A%2F%2Fcnrsf
> ormation.cnrs.fr%2Fstage.php%3Fstage%3D19089data=02%7C01%7Cjames.
> cline%40nist.gov%7Cb56878acaf134a6fdd5a08d640c58634%7C2ab5d82fd8fa4797
> a93e054655c61dec%7C1%7C0%7C636767614451670425sdata=aYdg0gg%2FhTWw
> hBPMBfn9u5lmxXKDwNh70ZDih8OOMNk%3Dreserved=0
> Formation SAXS et Réflectivités pour couches minces et matériaux 
> nanostructurés.
> https://na01.safelinks.protection.outlook.com/?url=https%3A%2F%2Fcnrsf
> ormation.cnrs.fr%2Fstage.php%3Fstage%3D19093data=02%7C01%7Cjames.
> cline%40nist.gov%7Cb56878acaf134a6fdd5a08d640c58634%7C2ab5d82fd8fa4797
> a93e054655c61dec%7C1%7C0%7C636767614451670425sdata=99Myif%2B0dBbc
> r1r8Plgg4y163Ma8RhxdKeE0nwbCl6k%3Dreserved=0
> Bibliographie
> https://na01.safelinks.protection.outlook.com/?url=https%3A%2F%2Fschol
> ar.google.fr%2Fcitations%3Fhl%3Dfr%26user%3DqC-lmN4J%26view_op%3Dl
> ist_works%26authuser%3D1%26sortby%3Dtitledata=02%7C01%7Cjames.cli
> ne%40nist.gov%7Cb56878acaf134a6fdd5a08d640c58634%7C2ab5d82fd8fa4797a93
> e054655c61dec%7C1%7C0%7C636767614451670425sdata=mjclfF1FR4s57RbKD
> Wxo44qGjopbhhQodIFwaFBP8jc%3Dreserved=0
> https://na01.safelinks.protection.outlook.com/?url=https%3A%2F%2Forcid
> .org%2F-0001-5339-3002data=02%7C01%7Cjames.cline%40nist.gov%7
> Cb56878acaf134a6fdd5a08d640c58634%7C2ab5d82fd8fa4797a93e054655c61dec%7
> C1%7C0%7C636767614451670425sdata=QNZFU9f7yP419SlmuOagzo18rGclVUVv
> dxeSExIH5A0%3Dreserved=0
>
>
>
> ---
> L'absence de virus dans ce courrier électronique a été vérifiée par le 
> logiciel antivirus Avast.
> https://na01.safelinks.protection.outlook.com/?url=https%3A%2F%2Fwww.a
> vast.com%2Fantivirusdata=02%7C01%7Cjames.cline%40nist.gov%7Cb5687
> 8acaf134a6fdd5a08d640c58634%7C2ab5d82fd8fa4797a93e054655c61dec%7C1%7C0
> %7C636767614451670425sdata=bepY%2FppDj96pLQ8j1swH8o2S%2BtyysqDg0O
> XEdCwVw2k%3Dreserved=0



--
Luzia S. Germann
Scientific Service Group Diffraction
Max-Planck-Institute for Solid State Research Heisenbergstr. 1
70569 Stuttgart
Germany

Phone: +49 711 689-1506

++
Please do NOT attach files to the whole list 
Send commands to  eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++



Re: Mixed refinement Topas example

2018-11-02 Thread Luzia Germann

Hey François,

You can find an example (with input file) on John's wonderful webpage  
under the following page:


http://community.dur.ac.uk/john.evans/topas_workshop/tutorial_combined.htm

There are also other, really cool tutorials, worth checking out!

Best,
Luzia

Quoting François Goutenoire :


Dear Rietveld users,

I am starting with Topas5.0 commercial, and I would like to do a  
mixed X-Ray-Neutron refinement directly on GUI mode.


Does anyone can send me an example of *.PRO file or even an *.INP  
file to to the refinement in launch mode.


The neutron data are with constant wavelength.

Thanks in advance.

--
*
Pr. Francois GOUTENOIRE
e-mail: francois.gouteno...@univ-lemans.fr
Tel: 02.43.83.33.54
FAX: 02.43.83.35.06
Skype Entreprise visio conférence
Département des Oxydes et Fluorures
Institut des Molécules et des Matériaux du Mans
IMMM - UMR CNRS 6283
Université du Maine - Avenue Olivier Messiaen
F-72085 Le Mans Cedex 9
FRANCE
*
Formation Rietveld CNRS 2019
https://cnrsformation.cnrs.fr/stage.php?stage=19089
Formation SAXS et Réflectivités pour couches minces et matériaux  
nanostructurés.

https://cnrsformation.cnrs.fr/stage.php?stage=19093
Bibliographie
https://scholar.google.fr/citations?hl=fr=qC-lmN4J_op=list_works=1=title
https://orcid.org/-0001-5339-3002



---
L'absence de virus dans ce courrier électronique a été vérifiée par  
le logiciel antivirus Avast.

https://www.avast.com/antivirus




--
Luzia S. Germann
Scientific Service Group Diffraction
Max-Planck-Institute for Solid State Research
Heisenbergstr. 1
70569 Stuttgart
Germany

Phone: +49 711 689-1506

++
Please do NOT attach files to the whole list 
Send commands to  eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++



Mixed refinement Topas example

2018-11-02 Thread François Goutenoire

Dear Rietveld users,

I am starting with Topas5.0 commercial, and I would like to do a mixed 
X-Ray-Neutron refinement directly on GUI mode.


Does anyone can send me an example of *.PRO file or even an *.INP file 
to to the refinement in launch mode.


The neutron data are with constant wavelength.

Thanks in advance.

--
*
Pr. Francois GOUTENOIRE
e-mail: francois.gouteno...@univ-lemans.fr
Tel: 02.43.83.33.54
FAX: 02.43.83.35.06
Skype Entreprise visio conférence
Département des Oxydes et Fluorures
Institut des Molécules et des Matériaux du Mans
IMMM - UMR CNRS 6283
Université du Maine - Avenue Olivier Messiaen
F-72085 Le Mans Cedex 9
FRANCE
*
Formation Rietveld CNRS 2019
https://cnrsformation.cnrs.fr/stage.php?stage=19089
Formation SAXS et Réflectivités pour couches minces et matériaux nanostructurés.
https://cnrsformation.cnrs.fr/stage.php?stage=19093
Bibliographie
https://scholar.google.fr/citations?hl=fr=qC-lmN4J_op=list_works=1=title
https://orcid.org/-0001-5339-3002



---
L'absence de virus dans ce courrier électronique a été vérifiée par le logiciel 
antivirus Avast.
https://www.avast.com/antivirus
++
Please do NOT attach files to the whole list 
Send commands to  eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++